Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

nozzle repad

Status
Not open for further replies.

mdischarge

Mechanical
Joined
Feb 21, 2006
Messages
9
Location
CA
for shell or head thickness over 40 mm , the repad should be integrally attached to the nozzle. any reason?
thanks
 
Well on a practical sense, the amount of heat from the weld you need to attach the re-pad can cause some distortion or the base metal to sink.
 
First off, is this a Code requirement? For some reason I don't recall this as a requirement.

Second - if this is not a code requirement it is a good practice to do because it provides additional load carrying capacity, and in my opinion increases resistance to failure from fatigue crack propagation in service.

The code only requires a fillet weld for the joint between the repad OD surface and the nozzle. However, I have seen fatigue crack propagation off the toe of this fillet weld into a nozzle, and have seen cracking that started from the nozzle/shell weld underneath the repad. This resulted in a leak thru the tell tale hole. I always require full penetration tie in between the repad and nozzle, with an external fillet weld, in lieu of only a fillet weld.
 