Is it possible to calculate a nozzle with double fillet weld (without full penetration) by Nozzle Pro?
I have a problem with it.
 
Sketch the actual cross-section of the weld in question: I think you're asking about an inside and an outside fillet weld of the same nozzle as it penetrates the tank wall.
 
bez_tytu%C5%82u_yvtadg.jpg
 