we are producing ring forgings from 4330. 11 1/32 x 9 21/32 x 2 21/32
after forging we need to Normalize can someone please suggest a cycle and temperatures and hours in furnace please.

thanks David
 
Review SAE AMS2359/1, Tables 2 and 5.
 
TVP- Did you mean AMS2759/1?

Tables 2 & 5 in AMS2759/1 provide temperature and soak time recommendations for normalize of 4330. Also be sure to pay attention to the notes and general requirements in the rest of the document.
 
Yes, that is supposed to be SAE AMS2759/1. Thanks for the clarification tbuelna.
 