Does anyone know where I can find Nitronic 33 fracture mechanics data? Is it superior or inferior to either Nitronic 40 or Nitronic 60?
 
In the annealed condition I would expect them to all be about the same. Only different by the strength levels.

In the cold worked condition I would expect 40 and 50 to be similar to each other, and better than 60 or 30/33.
30/33 are known to form some martensite on cold work and therefore would loose a bit of toughness esp at low temperatures.


= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 