I need some help in predicting shrinkage of pipe after it has been overlayed with nickel. I have a 30" long piece of 6" sch80 304ss pipe that will be overlayed with nickel. Any help will be appreciated. Bob
 
Replies continue below

Recommended for you

the overlay is NI99 0.125" thick. Bob
 
Please do not cross post, and see the response in
thread330-149098
 