Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Nickel Aluminium Bronze for Hydrocarbons

Status
Not open for further replies.

nickypaliwal

Materials
Joined
Aug 28, 2014
Messages
199
Location
OM
Is it allowed to use Nickel Aluminium Bronze or Aluminium Bronze for any type of hydrocarbons ? May it be benzene, naptha, crude oil etc.

is there any other fluid other than water, air and alkalies that aluminium bronze can handle ?

As below link from Copper association indicates use of Aluminium Bronze for various application however I have not generally come across its uses other than above mentioned.

 
I have seen NAB and AB used for refined hydrocarbons, but like all Cu alloys you never what to use them where there can be any exposure to H2S or free S.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
We used Nickel Aluminium Bronze for an automotive driveline application that was splashed with hydrocarbon gear lubricant (API GL-5).
 