Hello,
I want to find out the time it took x length of SA-210 steel to cool to a given temperature. Unfortunately I cannot get to my references as I am on travel. Does anyone have the equation to calculate that? If possible I would also like the coeff. of thermal expansion.
Thanks alot for the help,
Joe
 
The time to cool steel can be calculated assuming Newtonian Cooling using the Lumped Capacitance Method.

Coefficient of thermal expansion for SA 210 carbon steel boiler tubing is typically
~6.7 X 10^-6 in/in/deg F up to about 400 deg F.
 
Time also depends on how it's cooled, e.g., forced vs natural convection or conduction?