alehman
Electrical
- May 23, 1999
- 2,624
My client purchased a new pad-mounted (2500 kVA) transformer. It is installed but has not yet been energized and is leaking oil at one of the secondary bushings. The mfg. does not want the unit returned. Instead they want to have the bushing replaced in the field.
I recommended to my client that the manufacturer replace the unit or return it to the factory for repair. I am concerned about contamination, etc. from such work in the field. It's outdoors in an urban area, but not an especially dirty environment. Am I being overly cautious?