Is there correlation between Nernst equation and Pourbaix Diagram. Which one is better to determine corrosion rate /corrosion mechanism which probably occur in material?

Thanks and Regards,
ZA
 
Fontana's text is a classic.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
Corrosion is an interesting field, with nearly endless pits of quicksand to sink into.
Just remember, thermodynamics will tell you if a reaction is possible, but without know the rates you have no idea if it will actually happen.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
EdStainless said:
nearly endless pits of quicksand

I saw what you did there EdS!

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
I couldn't pass it up ...
The alternate is to fall into a crevice.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 
That would be very unpHortunate.