Does anyone know a Mil Spec or other widely accepted specification for bonding neoprene to metal?
 
Replies continue below

Recommended for you

Damc1,

Usually test specifications govern the testing method. To my knowledge there is no accepted specification describing bonding of any rubber to a metal surface. I suggest you contact a bonding agent supplier such as Lord Corp and ask them.

Graham.
 