Can any one give me the values of youngs modulus and tensile properties of SS420 ans 304SST.
What is the major difference between them. What does SST stand for.
Please help me. i despiratly need this information.

Thanks
Sarita
 
Replies continue below

Recommended for you

You can use 29,000,000psi for the young's modulus for both. maybe a little lower for the 304. Tensile properties vary widely for these two stainless steels depending on condition.


 
hi NickE,
Thanks for the information. so when i do structural analysis using this value. then how can the stress vary between them. so is the density different for both of them.
Actually i am doing a structural analysis using pro/e. so while defining the material, its asks for the density, thermal conductivity and the youngs modulus.
So can u give me further details regarding this.
And what can be a good source where i can find all such kind of details regarding metals.
PLease help me out.
Thanks
Sarita
 
420 is a martensitic stainless. Roughly 14% Cr with no Ni or Mo. It is hardenable by heat treatment, magnetic, and has limited corrosion resistance. The mechanical properties are a function of the heat treatment.
The room temp modulus is 30 million psi,
coef of thermal exp at room temp is 5.7 ppm/F,
the density is 0.276#/cuin,
and a thermal cond of 13.5 BTU/hr-ft-F.

304 is an austenitic stainless, roughly 18% Cr and 8% Ni. When annealed it is non-magnetic, very ductile and not very strong. This alloy can only be strengthened by cold working.
E rt = 28 million psi
CTE rt = 9.6 ppm/F
density = 0.287#/cuin
therm cond rt = 9.4 BTU/ft-hr-F

= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be managed.
 
SST means Stainless Steel.

You can obtain materials properties from MatWeb:


Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 