I cant seem to find any info on part number 5205T12-2RS
it is the T12 that is causing the problem. thanks for any help
 
Do you have a brand/manufacturer?
 
i think it may be IJK but can not find any thing in their catalog about (T12) the 12 may mean 3/4" boar?? the catalog says something about T standing for teflon seal but the 2RS we all know means rubber seals. im at a loss on this one, may have to request a sample from the customer.
 
Please provide measurements and brand name.

Russell Giuliano
 
well a 5205-2RS measures 25 X 52 X 20.6 But its the T12 that is throwing me off not the size. Thanks for the help, i will probebly request a sample from the customer. I just thought maybe someone here would know the answer.
 
For the record, T12 is a polymer cage material. So its just a standard sealed 5205 or 3205
 