Hi All
I'm buying some 316L Stainless steelplates to fabricate into pipes barrels then cut to suitable spool length and welded to form the discharge portion ( including tees and mitre bend) of a two large pumps system each pump handling 400000 cubic meter per day of municipal treated effluent( total 8 pumps) , pipe dia. from 1400 to 2200mm and thickness from 10 to 12mm . Fabrication to form pipe spools will be by rolling with stainless steel rollers to avoid contamination followed by either longitudinal weld or spiral weld . My question are as regard to the need for solution annealing
1)Would the rolling process of pipe forming cause sufficiently rigorous work hardening thus required some forms of heat treatment such as Solution annealing
2)Or is it because of the longitudinal Or Spiral weldings to form pipe barrel cause stress and embrittlement in the HAZ which then required solution annealing to dissolve carbon particle/precipitate in the HAZ,
3)If both activities in 1 & 2 are the cause for solution annealing, then which one is the main cause.
Solution annealing above is normally as follows :"heat to and soak for 5 minutes at 1040C, then air quenched in 5 minutes to 450C, then cool to ambient in 25~30 minutes".
Thanks you & look forward to your help.
Jyaces
I'm buying some 316L Stainless steelplates to fabricate into pipes barrels then cut to suitable spool length and welded to form the discharge portion ( including tees and mitre bend) of a two large pumps system each pump handling 400000 cubic meter per day of municipal treated effluent( total 8 pumps) , pipe dia. from 1400 to 2200mm and thickness from 10 to 12mm . Fabrication to form pipe spools will be by rolling with stainless steel rollers to avoid contamination followed by either longitudinal weld or spiral weld . My question are as regard to the need for solution annealing
1)Would the rolling process of pipe forming cause sufficiently rigorous work hardening thus required some forms of heat treatment such as Solution annealing
2)Or is it because of the longitudinal Or Spiral weldings to form pipe barrel cause stress and embrittlement in the HAZ which then required solution annealing to dissolve carbon particle/precipitate in the HAZ,
3)If both activities in 1 & 2 are the cause for solution annealing, then which one is the main cause.
Solution annealing above is normally as follows :"heat to and soak for 5 minutes at 1040C, then air quenched in 5 minutes to 450C, then cool to ambient in 25~30 minutes".
Thanks you & look forward to your help.
Jyaces