Need for a nose in foam pig / corrosion of metal components in pigs 1

Status
Not open for further replies.

Fred Sauna

Chemical
Joined
Oct 9, 2022
Messages
2
Location
OM
Hello. Can somebody explain why foam pigs have a pointed nose at the end?

Also, certain pigs have metal components in it (such as in articulated pigs or in the case of aluminum gauge plates). Is there not a possibility for these to be corroded by the process medium.

Thank you in advance.
 
I can see you are new here but have you spent too long in the sauna??

They have a pointed nose so that they know where to go. And makes it easier to launch and get over any obstacles.

Second one, no. Not in contact for long enough.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
What is the "process medium"? If its sulfuric acid you may be in trouble.
Put the pointy end in first.

Einstein gave the same test to students every year. When asked why he would do something like that, "Because the answers had changed."
 
Thanks, guys (binary term)... didn't know that.

So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
Not all foam pigs have noses. Some are flat nosed.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Let's keep this on track please.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Thanks everyone for your responses.

Can you please elaborate how the pointy nose helps in launching? I can see how it helps to overcome obstructions by breaking them apart.
 
Pig traps have a reducer from the big barrel to the pipeline size.

A pointy nose helps you to shove the pig in as far as you can into the pipeline sized bit so that it launches ok.

Remember - More details = better answers