Hi guys i would appreciate help looking for a polymer, ultem 1000 like, same ambar color, translucid, high tensile strength (more than 10000 psi). May be custom colored but translucid not opaque. Needs to be high impact resistent, but no fiber glass in it. Thank you for your hel
 
Replies continue below

Recommended for you

Thank you Pat for your help. I was looking to Polysulphone and it looks perfect. It looks just like ultem 1000. Do you know if Polysulphone is cheaper than Ultem 1000? Thanks again
 
Prices change by region and grade and with time, so I am not current.

You can ask suppliers of each for indicative costs. Both are aquite expensive.

Regards
Pat