Is there and alloy with similar mechanical strength properties of 6061-T6 that can widthstand heat better than it. We use 6061-T6 to make a tool that holds devices in an oven. Typical thickness of the tool is about 1/2" and L X W is around 6" X 6". The 6061-T6 is warping. I'm still trying to find out the actual temperature and time that the tool is in the oven, but can anyone recommend a different alloy? Currently can't switch from aluminum, and redesign of the tool is also not an option.

Thanks
 
In addition to 2618, alloys 2218, 2219 and 4032 are used at higher temperatures.
thread330-61426 discusses an Al-2%Mn-2%Ni cast alloy known as Pyral which is used in Europe for stove burners, etc.

Alcoa ( has a cast tooling plate called MIC-6 for which it claims several advantages, including thermal stability: "Thermal Cycling can be performed up to 800° F under controlled conditions." I believe that MIC-6 is similar to Al 6061 in composition.

Please explain whether the problem is warping (distortion upon change of T) or creep (slow distortion under load at high T).
 
Thanks for the responses. Unfortunately we may not be able to get a real clear awnser form our customer on how these parts warped.

I did find out however that the parts are placed in an over and slowed heated up to 250 C (482 F) and left for 72 hours. They are then left to cool to room temp for a day or so. Additionally these parts have been used for a couple years, and I'm guessing they were cycled once a week. Sounds to me more like a creep problem, but I'm no materials expert. Is there a way to tell by examining the parts (preferably without a microscope)?

Thanks again
 