Need adhesive to bond AlN to SS

Status
Not open for further replies.

Bluesky06

Electrical
Jul 27, 2006
2
I am in need of an adhesive to bond Aluminum nitride to stainless steel, and be capable of withstanding 300 degrees C. This will be used on a medical product so biocompatibility is a concern. Anyone have any ideas?
Thanks,
Fred
 
Replies continue below

Recommended for you

I would give these people a call.

This technology looks very promising compared to other methods to bond AlN to SS. The nanofoil is Nickel Aluminide. Bonding ceramics to CS/SS is a hot topic at the present time.

The only unknown is the biocompatibility.


 