I have got a small automatic MIG welding machine that is to be used in the field with a stick-out of 30 mm.
Problem is, from the moment everything is powered on (using a mobile generator), there is a certain arc voltage. The manufacturer gave a very useful gauge which can be used for several things, however as it is made out of Aluminum you cannot easily check the stick-out as it sparks heavily the moment you touch the torch (and the workpiece of course).
I want to have something small, handy, non-breakable (or relatively sturdy), and not electrically conducting that can handle temperatures of about 500 °C (930 Fahrenheit). Preferably easy to machine, and low-cost or good availibility.
I was thinking about bakelite, however I do not have any experience in plastics. Maybe there are better alternatives?
Other things that have crossed my mind:
Rock: ideal however cannot be shaped to form
Ceramics: too brittle.
Wood: probably my best bet so far. No problem if it won’t last long as it’s cheap and easy to acquire. Tolerance = +/- 1 mm, so when charred => bin and replace.
Thanks in advance for your input...
Problem is, from the moment everything is powered on (using a mobile generator), there is a certain arc voltage. The manufacturer gave a very useful gauge which can be used for several things, however as it is made out of Aluminum you cannot easily check the stick-out as it sparks heavily the moment you touch the torch (and the workpiece of course).
I want to have something small, handy, non-breakable (or relatively sturdy), and not electrically conducting that can handle temperatures of about 500 °C (930 Fahrenheit). Preferably easy to machine, and low-cost or good availibility.
I was thinking about bakelite, however I do not have any experience in plastics. Maybe there are better alternatives?
Other things that have crossed my mind:
Rock: ideal however cannot be shaped to form
Ceramics: too brittle.
Wood: probably my best bet so far. No problem if it won’t last long as it’s cheap and easy to acquire. Tolerance = +/- 1 mm, so when charred => bin and replace.
Thanks in advance for your input...