Good Afternoon,
I'm looking for standards that can be referenced to define NDT acceptance criteria for the following:
Rotating Shaft (Critical Component)
Material 4140
Test Specified - Ultrasonic Test and Liquid Penetrant Test
ASTM A788 (Standard Specification for Steel Forgings, General Requirements) does list criteria for UT, MPI, and LPT, however specifically states "Because of differences in manufacture, hot rolled, or hot rolled and cold finished bars (semi-finished or finished), billets or blooms are not considered to be forgings."
If the shaft was to be machined out of hot or colded rolled round bar, would this standard for acceptance criteria still be applicable or appropriate to apply? If not, are there any other ASTM standards that outline Classes of acceptance for bar (for UT, MPI, and LPT)? I have found an EN BS standard for UT of bars, but nothing from ASTM.
With regards to the A788 standard itself, what is the order of most stringent to least stringent UT level? I assume BR, DA, and then S.
Any comments with regards to what level's listed for acceptance are realistic?
Thanks
I'm looking for standards that can be referenced to define NDT acceptance criteria for the following:
Rotating Shaft (Critical Component)
Material 4140
Test Specified - Ultrasonic Test and Liquid Penetrant Test
ASTM A788 (Standard Specification for Steel Forgings, General Requirements) does list criteria for UT, MPI, and LPT, however specifically states "Because of differences in manufacture, hot rolled, or hot rolled and cold finished bars (semi-finished or finished), billets or blooms are not considered to be forgings."
If the shaft was to be machined out of hot or colded rolled round bar, would this standard for acceptance criteria still be applicable or appropriate to apply? If not, are there any other ASTM standards that outline Classes of acceptance for bar (for UT, MPI, and LPT)? I have found an EN BS standard for UT of bars, but nothing from ASTM.
With regards to the A788 standard itself, what is the order of most stringent to least stringent UT level? I assume BR, DA, and then S.
Any comments with regards to what level's listed for acceptance are realistic?