Mar 25, 2020 #1 adula29 Mechanical Joined Jul 10, 2009 Messages 53 Location PL Can we use GP240GH+QT as Killed carbon steel? This is selection for pump casing for petroleum industry.
Can we use GP240GH+QT as Killed carbon steel? This is selection for pump casing for petroleum industry.
Mar 25, 2020 #2 Guest I don't know, what does the material standard or norm say about it? "Everyone is entitled to their own opinions, but they are not entitled to their own facts." Upvote 0 Downvote
I don't know, what does the material standard or norm say about it? "Everyone is entitled to their own opinions, but they are not entitled to their own facts."
Mar 27, 2020 Thread starter #3 adula29 Mechanical Joined Jul 10, 2009 Messages 53 Location PL GP240GH+QT is EN-10213-2 Chemical composition % of steel GP240GH (1.0619): EN 10213-2007 C Si Mn Ni P S Cr Mo V Cu 0.18 - 0.23 max 0.6 0.5 - 1.2 max 0.4 max 0.03 max 0.02 max 0.3 max 0.12 max 0.03 max 0.3 Upvote 0 Downvote
GP240GH+QT is EN-10213-2 Chemical composition % of steel GP240GH (1.0619): EN 10213-2007 C Si Mn Ni P S Cr Mo V Cu 0.18 - 0.23 max 0.6 0.5 - 1.2 max 0.4 max 0.03 max 0.02 max 0.3 max 0.12 max 0.03 max 0.3
Mar 28, 2020 #4 SJones Petroleum Joined Apr 22, 2001 Messages 3,943 Location GB https://www.twi-global.com/technica...ls-made-using-different-deoxidation-practices Probably the wrong forum for the question. Try posting a closure statement and reposting in Metal & Metallurgy engineering. Steve Jones Corrosion Management Consultant http://www.linkedin.com/in/drstevejones All answers are personal opinions only and are in no way connected with any employer. Upvote 0 Downvote
https://www.twi-global.com/technica...ls-made-using-different-deoxidation-practices Probably the wrong forum for the question. Try posting a closure statement and reposting in Metal & Metallurgy engineering. Steve Jones Corrosion Management Consultant http://www.linkedin.com/in/drstevejones All answers are personal opinions only and are in no way connected with any employer.
Mar 31, 2020 #5 Guest Steve and the rest, There's been a rash of questions posted to incorrect forums recently. I encourage users to manage their personal forum lists. IM "Everyone is entitled to their own opinions, but they are not entitled to their own facts." Upvote 0 Downvote