Sep 11, 2013 #1 paulkersey Materials Joined Sep 11, 2013 Messages 2 Location US Is there a NACE spec that covers material requirements for Chemical Processing plants? (something similar to NACE MR0175 for Refineries?) Thank You.
Is there a NACE spec that covers material requirements for Chemical Processing plants? (something similar to NACE MR0175 for Refineries?) Thank You.
Sep 11, 2013 #2 bcd Mechanical Joined Sep 27, 2002 Messages 519 Location US NACE MR0103 Upvote 0 Downvote
Sep 11, 2013 Thread starter #3 paulkersey Materials Joined Sep 11, 2013 Messages 2 Location US Excuse me, MR0175 applies to downhole. MR0103-2012 is titled "Materials Resistant to Sulfide Stress Cracking in Corrosive Petroleum Refining Environments" Are you aware of a NACE standard similar (to MR0103) that applies to Chemical Processing environments? Thank You. Upvote 0 Downvote
Excuse me, MR0175 applies to downhole. MR0103-2012 is titled "Materials Resistant to Sulfide Stress Cracking in Corrosive Petroleum Refining Environments" Are you aware of a NACE standard similar (to MR0103) that applies to Chemical Processing environments? Thank You.
Sep 16, 2013 #4 pradipgoswami Materials Joined Jun 5, 2010 Messages 262 Location CA What specific chamical process environment you've in mind? There are API guidelines for broad based industries, same applies for NACE also. Both API and NACE has guidelines for various service environments. You need to be specific. Thanks. Pradip Goswami,P.Eng.IWE Welding & Metallurgical Specialist Ontario, Canada. ca.linkedin.com/pub/pradip-goswami/5/985/299 Upvote 0 Downvote
What specific chamical process environment you've in mind? There are API guidelines for broad based industries, same applies for NACE also. Both API and NACE has guidelines for various service environments. You need to be specific. Thanks. Pradip Goswami,P.Eng.IWE Welding & Metallurgical Specialist Ontario, Canada. ca.linkedin.com/pub/pradip-goswami/5/985/299