NACE MR0175 - Understanding The Requirements 1

Status
Not open for further replies.

AFG03082015

Mechanical
Jul 14, 2016
26
Hello,

Just wanted to check my understanding of NACE MR0175 correctly.

Am I right in saying NACE MR0175 is for materials to be used in sour environments that make the material susceptible to suplhide stress corrosion cracking?

Therefore, considering 17-4PH Precipitation Hardened Stainless Steel for example, the steel must have a Hardness limit of 33 HRC Age hardening at 620°C. This limit on the hardness therefore limits the materials susceptibility to stress corrosion cracking?
 
Replies continue below

Recommended for you

Yes you are right, amongst several other cracking mechanisms.

S17400 will be required to have a specific solution anneal followed by a double ageing, or modified double ageing, treatment.

Compliance gives some assurance of resistance to sulphide stress cracking/stress corrosion cracking, but it does not guarantee immunity.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 