Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

NACE MR0175/ISO 15156 (2009) compliance to Monel Casting M35-1 1

Status
Not open for further replies.

pawan797

Industrial
Joined
Feb 29, 2008
Messages
2
Location
IN
I am working in a Valve company and my customer is asking Monel casting M35-1 grade with NACE MR0175 (2009) compliance. Have read this standard and found nothing related to Monel M35-1 grade.

Older version of year 2000 specify compliance to MR0175 with max HRC 35 (hardness)

Can we certify Safety Relief Valve Body casting M35-1 (Monel) to NACE Mr0175/ISO 15156

 
Such certification cannot be provided with the above information for two reasons:

1. Compliance will depend upon detailed knowledge of the temperature, H2S partial pressure, chloride concentration, pH and elemental sulphur content of the fluid to which the material will be exposed

2. UNS N24315 is not listed in ISO 15156-3

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 