Good afternoon, everyone. I have a question regarding NACE MR0175 Part 3 A7.3
"A cross-section of the weld metal, HAZ and base metal shall be examined as part of the welding procedure qualification. The microstructure shall be suitably etched and examined at x400 magnification.... The ferrite content in the weld metal root and unreheated weld cap shall ve determined in accordance with ASTM E562 and shall be in the range of 30% to 70% volume fraction."
Does this apply to a 625 Ni alloy on a 2205 duplex base material? I am trying to get this passed through DNV and they are requesting me to include this in the testing. I don't see the purpose of looking for the ferrite in a 625 ni filler metal overlay.
What is your take?
Is there a code paragraph that I can give him to change his mind?
"A cross-section of the weld metal, HAZ and base metal shall be examined as part of the welding procedure qualification. The microstructure shall be suitably etched and examined at x400 magnification.... The ferrite content in the weld metal root and unreheated weld cap shall ve determined in accordance with ASTM E562 and shall be in the range of 30% to 70% volume fraction."
Does this apply to a 625 Ni alloy on a 2205 duplex base material? I am trying to get this passed through DNV and they are requesting me to include this in the testing. I don't see the purpose of looking for the ferrite in a 625 ni filler metal overlay.
What is your take?
Is there a code paragraph that I can give him to change his mind?