Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations Ron247 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

NACE MR0175 2015 Edition - Query on CRA

Status
Not open for further replies.

Bibek29

Mechanical
Sep 10, 2020
5
Question: Shall SDSS (UNS S32750) material (To be used at maximum temperature of 165 deg.C.) with H2S partial pressure 1.06 psi fall under the purview of NACE MR0175 2015?

 
Replies continue below

Recommended for you

Yes, it falls under acceptable range from Table A.24 of ISO-15156. Note that it shall be oxygen-free system.