Hi
Crude oil pipeline is sour and there are some storage tanks in terminal. Can we exclude NACE from these tanks? There is a table that exclude storage tanks in NACE MR 0175 but for flow lines not transportation pipelines.
 
Suggest You consider posting this question within the Petroleum Engineers and/or corrosion engineering forums

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 
I have this order where data sheet says heat tratement as per NACE requirement, Is post weld heat treatment necessary for Hatealloy C276(N10276) material necessary as per NACE MR175/ISO15156
 
PWHT is not necessary for this CRA.
 