rivtim

Automotive
Apr 7, 2006
17
I am quoting a threaded stud with these specifications. Any information would be appreciated.
 
Replies continue below

Recommended for you

All three are DaimlerChrysler Engineering Standards. MS-5479 specifies the requirements for carburized high-strength serrated studs. PS-6151 specified the identification requirements for metric fasteners, and PS-7099 is a general fastener specification. MS-5479 also references a number of other standards such as DCX PF-5188 and SAE J1102. DaimlerChrysler Engineering standards can be obtained directly from DCX via Covisint.
 