we are preparing a sample for a molded float in ebonite expanded capable of supporting a force of 1500 N m/sec.

May I ask any advise about the filler and the percentages to add for preserve the strengths inquired.

this type of manufacture is new for us we have ever produced only nr + s.

any advises could help me la lot

regards,

gl.volontà

 
I've only ever worked with solid rather than foamed ebonite. It is very brittle having a very high modulus and low elongation at break.
 
Our objective is to decrease the specific weight to allow the floating on liquids. the pure ebonite has a s.w. between 1,1-1,2 but if expanded the s.w goes down 1.
Otherwise for reduce the brittling we are adding 20 parts of ebonite dust on 100 of nr.