Can someone tell me if there is a similiar material in bar/rod.
 
Hold on. This is a different alloy.
M-30H is UNS N24030, 30% Cu, 3% Si, bal Ni. This is a cast grade under ASTM A494.

UNS 10001 is an age hardenable Ni-Mo alloy, not a cast grade. It is 30% Mo, bal Ni with some ageing elements added.
There are similar cast grades such as N30007, but as far as I remember they are not age hardenable. This grade is in A494 also.

= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be managed.
 
But if you look up A494 in the UNS Book it give a # UNS10001
 
I don't have that volume on hand. It shouldn't list N10001, it should have N30007 and N30012 as cast Ni-Mo alloys.
They probably dont have a common name, unless it is Alloy B.
The M-30H should be N24030 and a Ni-Cu chemistry.
If this isn't how the table reads is sounds like a editorial error. Are you looking at the -04 version of the spec?
I'll ask around and see if I can find a copy and help you sort this out.

= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be managed.
 
No, it's not the 04 copy. The only copy we have is my bossess copy and it looks like it is a couple years old. He advised me to use Hastaloy c276 solution an. to 60 min yield.
 
Hastelloy B UNS10001 is a solution strengthened Ni base superalloy from Haynes. According to my sources, it was supplied in cast form as A 494 Gr N-12MV. Not sure if Haynes would supply Hastelloy B because they recommend Haynes 242. Here is some technical information on the alloy;

 