Hi Everyone,

I am trying to model the transverse shear fracture within each ply of a composite ply. I am wondering if Abaqus has any built-in failure criteria that I can use to do this because the default Hashin damage criteria only accounts for in-plane ply failure. If not, then what can I do to add this failure mode to my model? Thank you.

ZhiMing
 
To clarify my question, I have implemented the Hashin failure criteria in Abaqus/Explicit to modeling failure of orthotropic materials. However, the criteria only account for in-plane failures (i.e. tension, compression, and shear) in the principle 1 and 2 directions. Is there a way to include failures in the out-of-plane directions as well? I would like to model the out-of-plane shear failure (for example, in direction 13) of an orthotropic material. Is this possible in Abaqus without writing my own user subroutines? Thank you very much.

ZhiMing
 
Status
Not open for further replies.