I'm trying to locate a material that I used to use that was produced by Mirafi and the material was called Miradrain (I think).
I cannot find a current listing for the material; it appears that Mirafi was bought out by someone.
The material is a polyethylene dimpled (about 1/2" deep dimples) sheet with a geotextile adhered to the one side and it provides a posiive drain against the wall surface. Does anyone have a link to it or to a similar product.
Dik
I cannot find a current listing for the material; it appears that Mirafi was bought out by someone.
The material is a polyethylene dimpled (about 1/2" deep dimples) sheet with a geotextile adhered to the one side and it provides a posiive drain against the wall surface. Does anyone have a link to it or to a similar product.