strainstress
Mechanical
- May 15, 2011
- 63
Table J2.4 of AISC ASD9th Edition provides minimum size of fillet welds. However they do not distinguish between lap joint or a t-joint. I would assume that Table is valid for only lapp joint fillet welds.
Is there any such minimum weld size table for T-joint fillet welds. I will be welding a 1/4" plate to 2" plate T-joint. Is there any minimum weld size that must be met to obtain a sound weld ?
Thanks
Is there any such minimum weld size table for T-joint fillet welds. I will be welding a 1/4" plate to 2" plate T-joint. Is there any minimum weld size that must be met to obtain a sound weld ?
Thanks