can anyone tell me the minimum size of a drilled shaft? Thanks.
 
I have a bit for my drill that is 1/8" diameter.

(sorry)

For drilled piers or auger cast piling, micro piling, etc. the minimum size probably depends upon what is available from your local drillers.

Well drillers can go to 4" I think.



 
haha! wiki says minimum is 18". I believe it.
 
There are a lot of types of bored piles. I have seen Franki expanded base piles with a shaft diameter of 350 mm, or about 14".
 
Auger cast piling - have seen them at 12" diameter. But again - just check with the local drillers to see what they can offer.

 
Based on my experience it is 18", but I even heard that contractors don't like them this small. We recently changed all our 18" shafts on a job to 24" just based on a contractor's recommendation on constructibility.
 
Auger Cast piling : 12"
Bored piles with bentonitic mud : 24" ( because of the size of the kelly bar )
 
When dealing with expansive soils, smaller is better, to reduce the uplift forces of the shaft side.
In Colorado I have seen thousand of residential projects with shafts of 8", 10" and 12". A lot of care is needed to construct these.
 
Call a local contractor and ask.

I have seen them down to 12"
 
We often use 12 or 16" dia in these environs... and about 30" dia for sleeve access.

Dik
 
In cases where the shaft is resting on rock, a downhole inspection is sometimes required. On these occasions it is good to be a large person.

30" min, 36" for the larger people. Reference FHWA - Drilled Shafts.
 
According to FHWA it can be as small as 12" but length should be limited to 8 to 10 feet. However, the document did not specify that a drill shaft cannot be less than 12". However, as a matter a practicality, I don't think it will be smaller.

 