Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Minimum Chamfer and/or Radius Edge Requirement For Brazing Steel Parts

Status
Not open for further replies.

TorsionalStress

Mechanical
Joined
May 23, 2005
Messages
234
Location
CA
I’m currently working on a design that requires the brazing of a steel insert into a groove of a mating steel part.

I would like to know if there is a rule of thumb or table that will provide the minimum edge chamfer and/or radius size on the steel insert for the best capillary attraction between parts?

Any response will be greatly appreciated!
 
I’m actually modifying a previous design which has a gap of 0.015” between the insert & mating part. After doing some research, I think this gap might be too large? Can anyone confirm?

Any response will be greatly appreciated!
 
Pretty sure that 15 mil is considered wide open in the brazing world. I've dealt with brazing nickel parts, and they require a 2-5 mil braze gap. Check the AWS Brazing Handbook - they have recommended gaps for different alloys.
 
This is why I asked, I also read (0.002 - 0.005”). The current insert is 0.375” fitting in a groove of 0.406”. I also think the fit dimensions have to be tighter?
 