Oct 9, 2012 #1 Redskinsdb21 Mining Joined May 4, 2009 Messages 45 Location US If I want to know how much Gold is being electroplated onto Carbon during an electroplating example, how would I calculate this? Use Faradays law or other techniques?
If I want to know how much Gold is being electroplated onto Carbon during an electroplating example, how would I calculate this? Use Faradays law or other techniques?
Oct 12, 2012 #2 metman Materials Joined Feb 18, 2002 Messages 1,187 Location US 1948 edition of Metals Handbook page 1107, "With 24-carat deposits, the weight laid down per ampere-hour may approach 7.3 g..." This is not in reference to any particular substrate such as Carbon. I don't know if this helps or not. Design for RELIABILITY, manufacturability, and maintainability Upvote 0 Downvote
1948 edition of Metals Handbook page 1107, "With 24-carat deposits, the weight laid down per ampere-hour may approach 7.3 g..." This is not in reference to any particular substrate such as Carbon. I don't know if this helps or not. Design for RELIABILITY, manufacturability, and maintainability