Mar 5, 2008 #1 fcochet Industrial Joined Oct 12, 2007 Messages 3 Location FR Who could tell me the minimum temperature admissible for ASTM A217 gr CA15. It seems that it is a equivalent to 410 but I am not sure. Thanks to help me.
Who could tell me the minimum temperature admissible for ASTM A217 gr CA15. It seems that it is a equivalent to 410 but I am not sure. Thanks to help me.
Mar 5, 2008 1 #2 arunmrao Materials Joined Oct 1, 2000 Messages 4,758 Location IN CA15 is a cast equivalent of 410 grade stainless steel. Save water Drink Beer Upvote 0 Downvote