May 8, 2003 #1 mohr New member Joined Dec 14, 2002 Messages 105 Location AR HELLO, Does anybody know where I could download the MIL-HDBK-5H handbook about metal characteristics) Any hell is very welcome Regards Mohr
HELLO, Does anybody know where I could download the MIL-HDBK-5H handbook about metal characteristics) Any hell is very welcome Regards Mohr
May 8, 2003 #2 kenvlach Materials Joined Apr 12, 2000 Messages 2,514 Location US The site for MIL & FED specs. is ASSIST-Quick Search at http://assist2.daps.dla.mil/quicksearch/ Note: MIL-HDBK-5H is 42 MB, and somewhere on this site is posted another site where you can download this particular spec. by section. Upvote 0 Downvote
The site for MIL & FED specs. is ASSIST-Quick Search at http://assist2.daps.dla.mil/quicksearch/ Note: MIL-HDBK-5H is 42 MB, and somewhere on this site is posted another site where you can download this particular spec. by section.
May 9, 2003 #3 swertel Mechanical Joined Dec 21, 2000 Messages 2,067 Location US To build onto kenvlach's note. Since the file is SO VERY BIG, and the assist download server is not very fast, consider downloading during low network traffic times and possibly using a download assistant. Upvote 0 Downvote
To build onto kenvlach's note. Since the file is SO VERY BIG, and the assist download server is not very fast, consider downloading during low network traffic times and possibly using a download assistant.
May 9, 2003 1 #4 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US MIL-HDBK-5 is available by chapter at the Granta Design website: http://www.grantadesign.com/cgi-bin/stat-tree.cgi?src=MIL5-H.xml&br=0 Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora. Upvote 0 Downvote
MIL-HDBK-5 is available by chapter at the Granta Design website: http://www.grantadesign.com/cgi-bin/stat-tree.cgi?src=MIL5-H.xml&br=0 Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
May 9, 2003 #5 kenvlach Materials Joined Apr 12, 2000 Messages 2,514 Location US A new revision, MIL-HDBK-5J METALLIC MATERIALS AND ELEMENTS FOR AEROSPACE VEHICLE STRUCTURES, is now available at the ASSIST site. Upvote 0 Downvote
A new revision, MIL-HDBK-5J METALLIC MATERIALS AND ELEMENTS FOR AEROSPACE VEHICLE STRUCTURES, is now available at the ASSIST site.