May 23, 2006 #1 mechnano Mechanical Joined May 5, 2006 Messages 28 Location KR hai Does any one know about the polishing paper used for fiber preform before microstructure study. Thanks
hai Does any one know about the polishing paper used for fiber preform before microstructure study. Thanks
May 23, 2006 1 #2 berkshire New member Joined Jun 8, 2005 Messages 4,429 Location US mechnano (Mechanical) Check with 3M and ask about their micro polishing paper,( It is actually on plastic film.) they have grades suitable for microscopic study. B.E. Upvote 0 Downvote
mechnano (Mechanical) Check with 3M and ask about their micro polishing paper,( It is actually on plastic film.) they have grades suitable for microscopic study. B.E.