I'm looking for sources for ceramic bearing vendors, and their use. Preferably in the USA. I have an application for a ceramic bearing in the neighborhood of .047" [1.2mm] ID bearing, .125" [3.2mm] L. All my search efforts are only churning up hits for RC cars and skateboards applications, I'm more interested in micro fan-like applications.

"Art without engineering is dreaming; Engineering without art is calculating."

Have you read faq731-376 to make the best use of these Forums?
 
Replies continue below

Recommended for you

You probably wont have much luck outside China for ceramic ball bearings. I got some for for 3mm shaft. Not very smooth.
With ceramic it is difficult to achieve the tolerances you can get with steel.

Jewel bearings might be a better option. A ruby plain bearing on metal spindle.

As ornerynorsk said. Bird Precision have a good range of jewel bearings.
 
Thanks for the lead. I should have been more specific, looking for plain sleeve bearings, not ball bearings. We hadn't considered jewels.

"Art without engineering is dreaming; Engineering without art is calculating."

Have you read faq731-376 to make the best use of these Forums?
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor