For a 9000 gallon methanol tank located at an oil & gas facility, what materials are recommended and why? We are considering carbon steel, or coated carbon steel. Apologies for the simple question - I am not a materials engineer.
 
Replies continue below

Recommended for you

ISO 21457 offers the option of carbon steel or 316 (L) stainless steel. Selection of the latter is normally down to product purity requirements for the stored methanol.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 