i am lookinf for a website that has a selection of Aluminium microstructures, particulary in the Heat treated condition. So far i have found nothing. Any help would be great.
 
Replies continue below

Recommended for you

So do I, but with the same result nothing.
I have some microphotographs for A356 before and after heat treat if you want I can send you.
I hope this will be a little help for you.
 
yeah please do, send them to Eric.clement@btinternet.com

thanks alot

 