Does anyone know where to find cross reference material specs for US materials in Russian or any European specs?

and/or

Possibly cross reference spec's of equivalent US materials in Russian or European materials?

Thanks
 
Replies continue below

Recommended for you

Check Stahl Schluessel on the web.
It is a cross reference for German,
European, and US Steels.
 
See the following thread for links to the best cross-referencing resources:

thread177-59325
 