Can any tell me or tell me where I can find the Modulus of Elasticity and the Specific Weight of F5 Alloy Steel at a temperature of 70 deg. F?
 
Are you referring to SA 182 F5 alloy steel?
 
Yes, F5 Alloy Steel - also referred to as 5 chrome, 1/2 moly. In particular, this would be 1 1/8" round barstock.
Thanks
 
Modulus at 70 deg F

31 X 10^6 psi

density;
0.27 lbs/in^3
 
donnaj - modulus at room temp is pretty much the same for all steels. 30x10^6 GPa

By specific weight do you mean density. You can usually use 7.87 g/cm^3.
 