Dear all,
For design consideration I need to know methanol catalyst particle density. Bulk density for this type of catalyst ranges between 1000-1250 Kg/M3, depending on the manufacturer of catalyst.
It would be appreciated if somebody can give me a figure and/or some references as guidline.
Thanks in advance.
 
I'm confused, don't you already have the range for the density?
 