Merus German Technology specially designed for Oil and Gas Industries’ infrastructure protection from Scaling, Corrosion & Bio Fouling in the Up & Down Streams. As you know that there are ever growing issues of Scaling, Corrosion, Fouling, Oil/water separation issues faced in days to day operations in Oil & Gas Industry; Merus technology is able to provide solutions to several problems as indicated below in the upstream and Downstream process and this technology is applicable right from the Downhole tubings to the refinery process. The beauty of the technology is that we do not require any Modification, Alterations or shutdown of an existing system.

Question: Do you think this technology will work fine in marine barge bilge system?
 
Replies continue below

Recommended for you

I have been impressed with German technology and manufacturing. This device, however, does not have any technology associated with it,

The merus ring is just another crackpot water gadget developed by some deluded inventor.

This device will not work on any application. There have been thousands of these gadgets sold by various marketing organizations over the years, and none of them work.

Do yourself a favor and through the brochure into the trash.




 