Anyone having trouble having Megalug Retainer Glands restrained joints on PVC water pipe passing hydrostatic pressure testing. I've had two jobs, one 16in CL 200 the other is 8 in CL 200 PVC. Only way we got the lines to pass is to back off the Megalug bolts to finger tight. Is there a better retainer?
 