Hello Everyone,
As per App.2 design of weld neck flange what is the governing thickness for MDMT???
g1,g0,t,(OD-ID)or some other thickness ???
Thanks
 
Replies continue below

Recommended for you

c8829, per UCS-66(a)(1)(a) thickness of the butt-weld, go. See also Fig UCS-66.3(c).