Hey
I have a Mazak laser 1300 W champion STX-48. Power is supposed to be 1300W but the average output power starts running at 500w and it keep on decreasing to 250w. Hence we are not able to cut anything on the laser. Can any one suggest what is the reason of the decline in the output power of the laser.
 
Replies continue below

Recommended for you

Don't double post- laser engineering is the right forum
 