Would anybody wish to comment on the bar spacings called out in 2003 IBC Tables 1805.5(2) to (4) as compared to ACI 318-02 Section 14.3.5?
Namely, the IBC prescribes bar spacings from 32" to 72" o.c. in their concrete foundation wall tables whereas ACI Chapter 14 says 18" o.c. maximum.
Since the IBC has more or less adopted the ACI, with some minor changes in IBC Chapter 19, where do they get these crazy (my subjective opinion) bar spacings?
Namely, the IBC prescribes bar spacings from 32" to 72" o.c. in their concrete foundation wall tables whereas ACI Chapter 14 says 18" o.c. maximum.
Since the IBC has more or less adopted the ACI, with some minor changes in IBC Chapter 19, where do they get these crazy (my subjective opinion) bar spacings?