Hello all.
I am a fairly new CWI, and have a question for anyone that can help. Where is D1.1 does it say the maximum amount of base metal that may be removed by grinding or any other means. I am thinking it will be a percentage of the base metal thickness, but can't seem to find it. 5.26 states that in a repair, "unacceptable portions of the weld shall be removed without substantial removal of the base metal." It doesn't say how much is substantial is. Any help is greatly appreciated. Ken
 
Hi emtrchr,
I'm fairly new to D1.1 myself, but C2.36.6.7 (2000) refers to toe grinding and a figure of 2mm or 5% of material thickness as being a limit.